Poland. Aluminium alloy

  • AI99,5E
  • AI99,8
  • AICu2SiMn
  • AICu4Mg2
  • AICuMg1
  • AIMg2
  • AIMg3
  • AIMg4.5Mn
  • AIMn1
  • AISi1MgMn
  • AISi7Mg
  • AISi9Mg
  • AIZn6Mg2Cu
  • Al99.7
  • AlCu2Mg2Ni1
  • AlMg5Si1
  • AlSi11
  • AlSi13Mg1CuNi
  • AlSiCu4