China. Stainless steel

  • 00Cr19Ni10
  • 00Cr19Ni11
  • 0Cr17Ni7Al
  • 0Cr18Ni11Nb
  • 0Cr18Ni11Ti
  • 0Cr18Ni12Mo3Ti
  • 0Cr19Ni9
  • 1Cr13
  • 1Cr15
  • 1Cr17
  • 1Cr17Ni2
  • 1Cr18Ni11Nb
  • 1Cr18Ni12Mo2Ti
  • 1Cr18Ni12Mo3Ti
  • 1Cr18Ni9
  • 1Cr18Ni9Ti
  • 1Cr19Ni11Nb
  • 1Cr25Ti
  • 2Cr13
  • 3Cr13
  • 4C13
  • ML1Cr17
  • ML1Cr17Ni2
  • OCr13
  • OCr18Ni10Ti
  • OCr18Ni12Mo2Ti
  • OCr18Ni9

  • China Stainless steel - equivalent grades