Equivalent grades   ->   USA. Aluminium alloy    

Equivalents to grade AA3004

    Country   -   USA         Standard   -   ANSI H35.2         Grade   -   AA3004    

    D12   ( Д12 )   -   Aluminium wrought alloys

  D12   ( Д12 ),      

D12   ( Д12 )   -   All Equivalent Grades
chemical composition, mechanical and technological properties

Types of delivery of grade D12   ( Д12 )
В54 - Ribbons


AA3004 USA Aluminium alloy:   Equivalent Grades for Russia, Ukraine, Belorussia, Kazakhstan...