Country - Germany | Standard - DIN 1709-1981 | Grade - G-CuZn25Al5 |
LTS23А6ZH3Mts2 ( ЛЦ23А6Ж3Мц2 ) - Cast cooper-zinc alloys LTS23А6ZH3Mts2 ( ЛЦ23А6Ж3Мц2 ), |
B51 - Non-ferrous metals, including rare metals, and their alloys |