Equivalents to grade C3710

    Country   -   Japan         Standard   -   JIS H3100         Grade   -   C3710    

NEW !  
SteelJIS : Free database of Japanese steels and alloys
SteelJIS.com contains the information about chemical composition and properties
more than 1400 Japanese engineering materials.
  SteelJIS.com:   Japanese Steels and Alloys



    LS60-1   ( ЛС60-1 )   -   Copper-zinc alloys pressure treated
    LS59-1   ( ЛС59-1 )   -   Copper-zinc alloys pressure treated

  LS60-1   ( ЛС60-1 ),         LS59-1   ( ЛС59-1 ),      

LS60-1   ( ЛС60-1 )   -   All Equivalent Grades
chemical composition, mechanical and technological properties

LS59-1   ( ЛС59-1 )   -   All Equivalent Grades
chemical composition, mechanical and technological properties

Types of delivery of grade LS59-1   ( ЛС59-1 )
B53 - Sheets and Strips
В54 - Ribbons
B55 - Bars
B64 - Pipes of non-ferrous metals and alloys
B74 - Wire made of non-ferrous metals and their alloys


C3710 Japan Latten (copper-zinc alloy):   Equivalent Grades for Russia, Ukraine, Belorussia, Kazakhstan...

    ©   2003 - 2019         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com
Рейтинг@Mail.ru