Equivalent grades   ->   USA. Copper    

Equivalents to grade C70400

    Country   -   USA         Standard   -   ASTM B466         Grade   -   C70400    

    MNZH5-1   ( МНЖ5-1 )   -   Copper-nickel alloys

  MNZH5-1   ( МНЖ5-1 ),      

MNZH5-1   ( МНЖ5-1 )   -   All Equivalent Grades
chemical composition, mechanical and technological properties

Types of delivery of grade MNZH5-1   ( МНЖ5-1 )
В05 - Welding and cutting of metals., Soldering, riveting
B51 - Non-ferrous metals, including rare metals, and their alloys
B64 - Pipes of non-ferrous metals and alloys


C70400 USA Copper:   Equivalent Grades for Russia, Ukraine, Belorussia, Kazakhstan...