Equivalents to grade H-99.95

    Country   -   Germany         Standard   -   DIN 17800         Grade   -   H-99.95    

    Mg95   ( Мг95 )   -   Primary magnesium

  Mg95   ( Мг95 ),      

Mg95   ( Мг95 )   -   All Equivalent Grades
chemical composition, mechanical and technological properties

Types of delivery of grade Mg95   ( Мг95 )
B51 - Non-ferrous metals, including rare metals, and their alloys


H-99.95 Germany Magnesium:   Equivalent Grades for Russia, Ukraine, Belorussia, Kazakhstan...