Equivalent grades   ->   USA. Titanium    

Equivalents to grade 4Al-3Mo-1V

    Country   -   USA         Standard   -   AMS 4912         Grade   -   4Al-3Mo-1V    

    VT14   ( ВТ14 )   -   Titanium wrought alloy

  VT14   ( ВТ14 ),      

VT14   ( ВТ14 )   -   All Equivalent Grades
chemical composition, mechanical and technological properties

Types of delivery of grade VT14   ( ВТ14 )
B53 - Sheets and Strips
B55 - Bars
В62 - Steel pipes and connecting parts to them


4Al-3Mo-1V USA Titanium:   Equivalent Grades for Russia, Ukraine, Belorussia, Kazakhstan...