Equivalents to grade 40NiCrMo6

    Country   -   Germany         Standard   -   DIN         Grade   -   40NiCrMo6    

    40KHN2MА   ( 40ХН2МА )   -   Alloy structurall steel
    40KH2N2MА   ( 40Х2Н2МА )   -   Alloy structurall steel

  40KHN2MА   ( 40ХН2МА ),         40KH2N2MА   ( 40Х2Н2МА ),      

40KHN2MА   ( 40ХН2МА )   -   All Equivalent Grades
chemical composition, mechanical and technological properties

Types of delivery of grade 40KHN2MА   ( 40ХН2МА )
B03 - Metal forming treatment. Forgings
В22 - Graded and shaped rolling
B23 - Sheets and Strips
В32 - Graded and shaped rolling
В71 - Low-carbon steel wire

40KH2N2MА   ( 40Х2Н2МА )   -   All Equivalent Grades
chemical composition, mechanical and technological properties

Types of delivery of grade 40KH2N2MА   ( 40Х2Н2МА )
B03 - Metal forming treatment. Forgings
В22 - Graded and shaped rolling
B23 - Sheets and Strips
В32 - Graded and shaped rolling


40NiCrMo6 Germany Structural steel:   Equivalent Grades for Russia, Ukraine, Belorussia, Kazakhstan...