Equivalent grades   ->   China. Stainless steel    

Equivalents to grade 2Cr13

    Country   -   China         Standard   -   GB 1220-92         Grade   -   2Cr13    

    20KH13   ( 20Х13 )   -   Corrosion-resistant high-temperature steel
    12KH13   ( 12Х13 )   -   Corrosion-resistant high-temperature steel

  20KH13   ( 20Х13 ),         12KH13   ( 12Х13 ),      

20KH13   ( 20Х13 )   -   All Equivalent Grades
chemical composition, mechanical and technological properties

Types of delivery of grade 20KH13   ( 20Х13 )
B03 - Metal forming treatment. Forgings
В22 - Graded and shaped rolling
B23 - Sheets and Strips
В32 - Graded and shaped rolling
B33 - Sheets and Strips
B34 - Ribbons
В62 - Steel pipes and connecting parts to them
B73 - Steel Alloy Wire
B76 - Metal nets

12KH13   ( 12Х13 )   -   All Equivalent Grades
chemical composition, mechanical and technological properties

Types of delivery of grade 12KH13   ( 12Х13 )
B03 - Metal forming treatment. Forgings
В22 - Graded and shaped rolling
B23 - Sheets and Strips
В32 - Graded and shaped rolling
B33 - Sheets and Strips
B34 - Ribbons
В62 - Steel pipes and connecting parts to them
B73 - Steel Alloy Wire
B76 - Metal nets


2Cr13 China Stainless steel:   Equivalent Grades for Russia, Ukraine, Belorussia, Kazakhstan...