Country - England | Standard - BS 1429 | Grade - 070A72 |
70 ( 70 ) - Spring structural steel 75 ( 75 ) - Spring structural steel 70 ( 70 ), 75 ( 75 ), |
В22 - Graded and shaped rolling |
B23 - Sheets and Strips |
В32 - Graded and shaped rolling |
B33 - Sheets and Strips |
B34 - Ribbons |
В71 - Low-carbon steel wire |
В72 - Medium-high and high-carbon steel wire |
В22 - Graded and shaped rolling |
B23 - Sheets and Strips |
В32 - Graded and shaped rolling |
B33 - Sheets and Strips |
В72 - Medium-high and high-carbon steel wire |