Equivalents to grade C55

    Country   -   England         Standard   -   BS EN 10083-2         Grade   -   C55    

    55   ( 55 )   -   High quality structural carbon steel
    50   ( 50 )   -   High quality structural carbon steel

  55   ( 55 ),         50   ( 50 ),      

55   ( 55 )   -   All Equivalent Grades
chemical composition, mechanical and technological properties

Types of delivery of grade 55   ( 55 )
B03 - Metal forming treatment. Forgings
В22 - Graded and shaped rolling
B23 - Sheets and Strips
B24 - Ribbons
В32 - Graded and shaped rolling
B33 - Sheets and Strips
B34 - Ribbons
В62 - Steel pipes and connecting parts to them
В71 - Low-carbon steel wire
В72 - Medium-high and high-carbon steel wire
B76 - Metal nets

50   ( 50 )   -   All Equivalent Grades
chemical composition, mechanical and technological properties

Types of delivery of grade 50   ( 50 )
B03 - Metal forming treatment. Forgings
В05 - Welding and cutting of metals., Soldering, riveting
В22 - Graded and shaped rolling
B23 - Sheets and Strips
B24 - Ribbons
В32 - Graded and shaped rolling
B33 - Sheets and Strips
B34 - Ribbons
В62 - Steel pipes and connecting parts to them
В71 - Low-carbon steel wire
В72 - Medium-high and high-carbon steel wire
B76 - Metal nets


C55 England Structural steel:   Equivalent Grades for Russia, Ukraine, Belorussia, Kazakhstan...

    ©   2003 - 2024         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru