Country - China | Standard - GB/T 3077-88 | Grade - 30Mn2 |
30G2 ( 30Г2 ) - Alloy structurall steel 30G ( 30Г ) - Alloy structurall steel 30GSL ( 30ГСЛ ) - Casting alloy steel for general purposes 30G2 ( 30Г2 ), 30G ( 30Г ), 30GSL ( 30ГСЛ ), |
В22 - Graded and shaped rolling |
B23 - Sheets and Strips |
В32 - Graded and shaped rolling |
В22 - Graded and shaped rolling |
B23 - Sheets and Strips |
В32 - Graded and shaped rolling |
B33 - Sheets and Strips |
B82 - Steel Castings |