Database of Steel and Alloy (Marochnik) |
Home | Steel and Alloy | Search | Equivalent Grades | GOST Standards | Grading | Contacts |
Country - France | Standard - AFNOR NF A 35-571 | Grade - 45C4 |
45KH ( 45Х ) - Alloy structurall steel 50KHG ( 50ХГ ) - Spring structural steel 45KH ( 45Х ), 50KHG ( 50ХГ ), |
B03 - Metal forming treatment. Forgings |
В22 - Graded and shaped rolling |
B23 - Sheets and Strips |
В32 - Graded and shaped rolling |
B33 - Sheets and Strips |
В71 - Low-carbon steel wire |
В22 - Graded and shaped rolling |
B23 - Sheets and Strips |
В32 - Graded and shaped rolling |
B33 - Sheets and Strips |
В72 - Medium-high and high-carbon steel wire |
© 2003 - 2024 Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use. |