Database of Steel and Alloy (Marochnik)

  Home     Steel and Alloy     Search     Equivalent Grades     GOST Standards     Grading     Contacts  
         
Equivalent grades   ->   France. High-temperature or heat-resistant steel and alloy    

Equivalents to grade Z6CNDNB17-12

    Country   -   France         Standard   -   AFNOR NF         Grade   -   Z6CNDNB17-12    

    08KH16N13M2B   ( 08Х16Н13М2Б )   -   High alloy high-temperature steel

  08KH16N13M2B   ( 08Х16Н13М2Б ),      

08KH16N13M2B   ( 08Х16Н13М2Б )   -   All Equivalent Grades
chemical composition, mechanical and technological properties

Types of delivery of grade 08KH16N13M2B   ( 08Х16Н13М2Б )
В22 - Graded and shaped rolling
B23 - Sheets and Strips
В32 - Graded and shaped rolling
B33 - Sheets and Strips


Z6CNDNB17-12 France High-temperature or heat-resistant steel and alloy:   Equivalent Grades for Russia, Ukraine, Belorussia, Kazakhstan...

    ©   2003 - 2019         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com
Рейтинг@Mail.ru