Equivalents to grade Z3CND17-12-03

    Country   -   France         Standard   -   AFNOR NF         Grade   -   Z3CND17-12-03    

    03KH17N14M3   ( 03Х17Н14М3 )   -   Сryogenic structural steel
    03KH16N15M3   ( 03Х16Н15М3 )   -   Corrosion-resistant steel for general purposes

  03KH17N14M3   ( 03Х17Н14М3 ),         03KH16N15M3   ( 03Х16Н15М3 ),      

03KH17N14M3   ( 03Х17Н14М3 )   -   All Equivalent Grades
chemical composition, mechanical and technological properties

Types of delivery of grade 03KH17N14M3   ( 03Х17Н14М3 )
B03 - Metal forming treatment. Forgings
В22 - Graded and shaped rolling
B23 - Sheets and Strips
В32 - Graded and shaped rolling
B33 - Sheets and Strips
В62 - Steel pipes and connecting parts to them

03KH16N15M3   ( 03Х16Н15М3 )   -   All Equivalent Grades
chemical composition, mechanical and technological properties


Z3CND17-12-03 France Stainless steel:   Equivalent Grades for Russia, Ukraine, Belorussia, Kazakhstan...

    ©   2003 - 2019         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com
Рейтинг@Mail.ru