    Country   -   Czechia         Standard   -   CSN         Grade   -   17041    

    08KH17T   ( 08Х17Т )   -   Corrosion-resistant high-temperature steel
    12KH17   ( 12Х17 )   -   Corrosion-resistant high-temperature steel

  08KH17T   ( 08Х17Т ),         12KH17   ( 12Х17 ),      

08KH17T   ( 08Х17Т )   -   All Equivalent Grades
chemical composition, mechanical and technological properties

Types of delivery of grade 08KH17T   ( 08Х17Т )
В22 - Graded and shaped rolling
B23 - Sheets and Strips
В32 - Graded and shaped rolling
B33 - Sheets and Strips
В62 - Steel pipes and connecting parts to them

12KH17   ( 12Х17 )   -   All Equivalent Grades
chemical composition, mechanical and technological properties

Types of delivery of grade 12KH17   ( 12Х17 )
В22 - Graded and shaped rolling
B23 - Sheets and Strips
В32 - Graded and shaped rolling
B33 - Sheets and Strips
В62 - Steel pipes and connecting parts to them


17041 Czechia Stainless steel:   Equivalent Grades for Russia, Ukraine, Belorussia, Kazakhstan...

    ©   2003 - 2019         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com
Рейтинг@Mail.ru