    Country   -   Spain         Standard   -   UNE         Grade   -   F.1203    

    35G2   ( 35Г2 )   -   Alloy structurall steel
    35GL   ( 35ГЛ )   -   Casting alloy steel for general purposes

  35G2   ( 35Г2 ),         35GL   ( 35ГЛ ),      

35G2   ( 35Г2 )   -   All Equivalent Grades
chemical composition, mechanical and technological properties

Types of delivery of grade 35G2   ( 35Г2 )
B03 - Metal forming treatment. Forgings
В22 - Graded and shaped rolling
B23 - Sheets and Strips
В32 - Graded and shaped rolling
B33 - Sheets and Strips
В71 - Low-carbon steel wire

35GL   ( 35ГЛ )   -   All Equivalent Grades
chemical composition, mechanical and technological properties

Types of delivery of grade 35GL   ( 35ГЛ )
B82 - Steel Castings


F.1203 Spain Casting steel:   Equivalent Grades for Russia, Ukraine, Belorussia, Kazakhstan...

    ©   2003 - 2019         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com
Рейтинг@Mail.ru