Equivalents to grade SCM432

    Country   -   Japan         Standard   -   JIS G4105         Grade   -   SCM432    

NEW !  
SteelJIS : Free database of Japanese steels and alloys
SteelJIS.com contains the information about chemical composition and properties
more than 1400 Japanese engineering materials.
  SteelJIS.com:   Japanese Steels and Alloys



    30KhMА   ( 30ХМА )   -   Relaxation-resistant steel
    АS38KHGM   ( АС38ХГМ )   -   Rolled steel of improved and high cutting machinability
    35KhM   ( 35ХМ )   -   Relaxation-resistant steel
    35KHML   ( 35ХМЛ )   -   Casting alloy steel for general purposes
    30KhM   ( 30ХМ )   -   Relaxation-resistant steel

  30KhMА   ( 30ХМА ),         АS38KHGM   ( АС38ХГМ ),         35KhM   ( 35ХМ ),         35KHML   ( 35ХМЛ ),         30KhM   ( 30ХМ ),      

30KhMА   ( 30ХМА )   -   All Equivalent Grades
chemical composition, mechanical and technological properties

Types of delivery of grade 30KhMА   ( 30ХМА )
B03 - Metal forming treatment. Forgings
В22 - Graded and shaped rolling
B23 - Sheets and Strips
В32 - Graded and shaped rolling
В62 - Steel pipes and connecting parts to them
В71 - Low-carbon steel wire

АS38KHGM   ( АС38ХГМ )   -   All Equivalent Grades
chemical composition, mechanical and technological properties

Types of delivery of grade АS38KHGM   ( АС38ХГМ )
В22 - Graded and shaped rolling
В32 - Graded and shaped rolling

35KhM   ( 35ХМ )   -   All Equivalent Grades
chemical composition, mechanical and technological properties

Types of delivery of grade 35KhM   ( 35ХМ )
B03 - Metal forming treatment. Forgings
В22 - Graded and shaped rolling
B23 - Sheets and Strips
В32 - Graded and shaped rolling

35KHML   ( 35ХМЛ )   -   All Equivalent Grades
chemical composition, mechanical and technological properties

Types of delivery of grade 35KHML   ( 35ХМЛ )
B82 - Steel Castings
B83 - Castings with special properties (cast iron and steel)

30KhM   ( 30ХМ )   -   All Equivalent Grades
chemical composition, mechanical and technological properties

Types of delivery of grade 30KhM   ( 30ХМ )
B03 - Metal forming treatment. Forgings
В22 - Graded and shaped rolling
B23 - Sheets and Strips
В32 - Graded and shaped rolling


SCM432 Japan High-temperature or heat-resistant steel and alloy:   Equivalent Grades for Russia, Ukraine, Belorussia, Kazakhstan...

    ©   2003 - 2019         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com
Рейтинг@Mail.ru