Database of Steel and Alloy (Marochnik) |
Home | Steel and Alloy | Search | Equivalent Grades | GOST Standards | Grading | Contacts |
Country - Japan | Standard - JIS | Grade - SCMn3 |
35G2 ( 35Г2 ) - Alloy structurall steel 35GL ( 35ГЛ ) - Casting alloy steel for general purposes 35G2 ( 35Г2 ), 35GL ( 35ГЛ ), |
B03 - Metal forming treatment. Forgings |
В22 - Graded and shaped rolling |
B23 - Sheets and Strips |
В32 - Graded and shaped rolling |
B33 - Sheets and Strips |
В71 - Low-carbon steel wire |
B82 - Steel Castings |