Equivalent grades   ->   Poland. Structural steel    

Equivalents to grade G355

    Country   -   Poland         Standard   -   PN H-74244         Grade   -   G355    

    S345   ( С345 )   -   Steel for structural constructions
    17G1S   ( 17Г1С )   -   Structural steel for welding construct
    17GS   ( 17ГС )   -   Structural steel for welding construct

  S345   ( С345 ),         17G1S   ( 17Г1С ),         17GS   ( 17ГС ),      

S345   ( С345 )   -   All Equivalent Grades
chemical composition, mechanical and technological properties

Types of delivery of grade S345   ( С345 )
В22 - Graded and shaped rolling
B23 - Sheets and Strips

17G1S   ( 17Г1С )   -   All Equivalent Grades
chemical composition, mechanical and technological properties

Types of delivery of grade 17G1S   ( 17Г1С )
В22 - Graded and shaped rolling
B23 - Sheets and Strips
B33 - Sheets and Strips
В62 - Steel pipes and connecting parts to them

17GS   ( 17ГС )   -   All Equivalent Grades
chemical composition, mechanical and technological properties

Types of delivery of grade 17GS   ( 17ГС )
В22 - Graded and shaped rolling
B23 - Sheets and Strips
B33 - Sheets and Strips
В62 - Steel pipes and connecting parts to them


G355 Poland Structural steel:   Equivalent Grades for Russia, Ukraine, Belorussia, Kazakhstan...

    ©   2003 - 2019         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com
Рейтинг@Mail.ru