Equivalents to grade Gr.50

    Country   -   USA         Standard   -   AISI         Grade   -   Gr.50    

    S285   ( С285 )   -   Steel for structural constructions

  S285   ( С285 ),      

S285   ( С285 )   -   All Equivalent Grades
chemical composition, mechanical and technological properties

Types of delivery of grade S285   ( С285 )
В22 - Graded and shaped rolling
B23 - Sheets and Strips


Gr.50 USA Steel for special use:   Equivalent Grades for Russia, Ukraine, Belorussia, Kazakhstan...