Equivalents to grade St5

    Country   -   Poland         Standard   -   PN/H 84020         Grade   -   St5    

    S285   ( С285 )   -   Steel for structural constructions
    St5ps   ( Ст5пс )   -   Normal quality structural carbon steel
    St5sp   ( Ст5сп )   -   Normal quality structural carbon steel

  S285   ( С285 ),         St5ps   ( Ст5пс ),         St5sp   ( Ст5сп ),      

S285   ( С285 )   -   All Equivalent Grades
chemical composition, mechanical and technological properties

Types of delivery of grade S285   ( С285 )
В22 - Graded and shaped rolling
B23 - Sheets and Strips

St5ps   ( Ст5пс )   -   All Equivalent Grades
chemical composition, mechanical and technological properties

Types of delivery of grade St5ps   ( Ст5пс )
B03 - Metal forming treatment. Forgings
В20 - Classification, nomenclature and general norms
В22 - Graded and shaped rolling
B23 - Sheets and Strips
B24 - Ribbons
B42 - Rails: Pads, Pads, Crutches
В62 - Steel pipes and connecting parts to them

St5sp   ( Ст5сп )   -   All Equivalent Grades
chemical composition, mechanical and technological properties

Types of delivery of grade St5sp   ( Ст5сп )
B03 - Metal forming treatment. Forgings
В20 - Classification, nomenclature and general norms
В22 - Graded and shaped rolling
B23 - Sheets and Strips
B24 - Ribbons
B42 - Rails: Pads, Pads, Crutches
В62 - Steel pipes and connecting parts to them


St5 Poland Structural steel:   Equivalent Grades for Russia, Ukraine, Belorussia, Kazakhstan...

    ©   2003 - 2019         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com
Рейтинг@Mail.ru