Equivalents to grade 422992

    Country   -   Czechia         Standard   -   CSN         Grade   -   422992    

    R9   ( Р9 )   -   High speed tool steel

  R9   ( Р9 ),      

R9   ( Р9 )   -   All Equivalent Grades
chemical composition, mechanical and technological properties

Types of delivery of grade R9   ( Р9 )
B34 - Ribbons


422992 Czechia Tool steel:   Equivalent Grades for Russia, Ukraine, Belorussia, Kazakhstan...