Database of Steel and Alloy (Marochnik) |
Home | Steel and Alloy | Search | Equivalent Grades | GOST Standards | Grading | Contacts |
Country - Germany | Standard - DIN 17350 | Grade - X210CrW12 |
KH12VM ( Х12ВМ ) - Die tool steel KH12 ( Х12 ) - Die tool steel KH12VMF ( Х12ВМФ ) - Die tool steel KH12VM ( Х12ВМ ), KH12 ( Х12 ), KH12VMF ( Х12ВМФ ), |
В32 - Graded and shaped rolling |
В32 - Graded and shaped rolling |