Equivalents to grade 1.4305

Warning! Indicated both exact and nearest equivalents
    Country   -   Germany         Standard   -   WNr         Grade   -   1.4305    

    12KH18N9 ( 12Х18Н9 )   -   Corrosion-resistant high-temperature steel

  12KH18N9 ( 12Х18Н9 ),      

1.4305 Germany Stainless steel - equivalent grades