Equivalent grades   ->   France. Stainless steel    

Equivalents to grade Z8CNA17-07

    Country   -   France         Standard   -   AFNOR NF         Grade   -   Z8CNA17-07    

    09KH17N7YU1   ( 09Х17Н7Ю1 )   -   Corrosion-resistant steel for general purposes

  09KH17N7YU1   ( 09Х17Н7Ю1 ),      

09KH17N7YU1   ( 09Х17Н7Ю1 )   -   All Equivalent Grades
chemical composition, mechanical and technological properties

Types of delivery of grade 09KH17N7YU1   ( 09Х17Н7Ю1 )
В22 - Graded and shaped rolling
B23 - Sheets and Strips
В32 - Graded and shaped rolling
B33 - Sheets and Strips


Z8CNA17-07 France Stainless steel:   Equivalent Grades for Russia, Ukraine, Belorussia, Kazakhstan...

    ©   2003 - 2019         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com
Рейтинг@Mail.ru