Equivalents to grade N13

    Country   -   Poland         Standard   -   PN/H 85020         Grade   -   N13    

    U13   ( У13 )   -   Carbon tool steel

  U13   ( У13 ),      

U13   ( У13 )   -   All Equivalent Grades
chemical composition, mechanical and technological properties

Types of delivery of grade U13   ( У13 )