Equivalents to grade STKM19C

    Country   -   Japan         Standard   -   JIS G 3445         Grade   -   STKM19C    

NEW !  
SteelJIS : Free database of Japanese steels and alloys
SteelJIS.com contains the information about chemical composition and properties
more than 1400 Japanese engineering materials.
  SteelJIS.com:   Japanese Steels and Alloys



    St4ps   ( Ст4пс )   -   Normal quality structural carbon steel

  St4ps   ( Ст4пс ),      

St4ps   ( Ст4пс )   -   All Equivalent Grades
chemical composition, mechanical and technological properties

Types of delivery of grade St4ps   ( Ст4пс )
В20 - Classification, nomenclature and general norms
В22 - Graded and shaped rolling
B23 - Sheets and Strips
B24 - Ribbons
B42 - Rails: Pads, Pads, Crutches
В62 - Steel pipes and connecting parts to them


STKM19C Japan Structural steel:   Equivalent Grades for Russia, Ukraine, Belorussia, Kazakhstan...

    ©   2003 - 2024         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru