    YOU HERE:   Equivalent grades   ->   Japan. Structural steel    

Equivalents to grade S10C

Warning! Indicated both exact and nearest equivalents
    Country   -   Japan         Standard   -   JIS G4051         Grade   -   S10C    

    10 ( 10 )   -   High quality structural carbon steel
    08 ( 08 )   -   High quality structural carbon steel

  10 ( 10 ),         08 ( 08 ),      

S10C Japan Structural steel - equivalent grades