Equivalents to grade 40H2MF

    Country   -   Poland         Standard   -   PN/H 84030         Grade   -   40H2MF    

    40KHMFА   ( 40ХМФА )   -   Alloy structurall steel

  40KHMFА   ( 40ХМФА ),      

40KHMFА   ( 40ХМФА )   -   All Equivalent Grades
chemical composition, mechanical and technological properties

Types of delivery of grade 40KHMFА   ( 40ХМФА )
В22 - Graded and shaped rolling
B23 - Sheets and Strips
В32 - Graded and shaped rolling


40H2MF Poland Structural steel:   Equivalent Grades for Russia, Ukraine, Belorussia, Kazakhstan...