Database of Steel and Alloy (Marochnik) |
Home | Steel and Alloy | Search | Equivalent Grades | GOST Standards | Grading | Contacts |
Country - South Korea | Standard - KS D 4103 | Grade - SSC12 |
10KH18N9L ( 10Х18Н9Л ) - Casting alloy steel with specific properties 12KH18N9TL ( 12Х18Н9ТЛ ) - Casting alloy steel with specific properties 10KH18N9L ( 10Х18Н9Л ), 12KH18N9TL ( 12Х18Н9ТЛ ), |
B82 - Steel Castings |
B82 - Steel Castings |