Database of Steel and Alloy (Marochnik)

  Home     Steel and Alloy     Search     Equivalent Grades     GOST Standards     Grading     Contacts  
         
Equivalent grades   ->   Germany. Tool steel    

Equivalents to grade 45WCrV7

    Country   -   Germany         Standard   -   DIN         Grade   -   45WCrV7    

    5KHV2S   ( 5ХВ2С )   -   Die tool steel
    5KHV2SF   ( 5ХВ2СФ )   -   Alloy tool steel
    4KH4VMFS   ( 4Х4ВМФС )   -   Die tool steel
    3KH3M3F   ( 3Х3М3Ф )   -   Die tool steel

  5KHV2S   ( 5ХВ2С ),         5KHV2SF   ( 5ХВ2СФ ),         4KH4VMFS   ( 4Х4ВМФС ),         3KH3M3F   ( 3Х3М3Ф ),      

5KHV2S   ( 5ХВ2С )   -   All Equivalent Grades
chemical composition, mechanical and technological properties

Types of delivery of grade 5KHV2S   ( 5ХВ2С )
В22 - Graded and shaped rolling
B31 - Blanks, Blanks, Slabs
В32 - Graded and shaped rolling
B33 - Sheets and Strips

5KHV2SF   ( 5ХВ2СФ )   -   All Equivalent Grades
chemical composition, mechanical and technological properties

Types of delivery of grade 5KHV2SF   ( 5ХВ2СФ )
В32 - Graded and shaped rolling

4KH4VMFS   ( 4Х4ВМФС )   -   All Equivalent Grades
chemical composition, mechanical and technological properties

Types of delivery of grade 4KH4VMFS   ( 4Х4ВМФС )
В32 - Graded and shaped rolling

3KH3M3F   ( 3Х3М3Ф )   -   All Equivalent Grades
chemical composition, mechanical and technological properties

Types of delivery of grade 3KH3M3F   ( 3Х3М3Ф )
В22 - Graded and shaped rolling
B31 - Blanks, Blanks, Slabs
В32 - Graded and shaped rolling
B33 - Sheets and Strips


45WCrV7 Germany Tool steel:   Equivalent Grades for Russia, Ukraine, Belorussia, Kazakhstan...

    ©   2003 - 2024         Database of Steel and Alloy (russian title is the Marochnik)