Country - USA | Standard - UNS | Grade - S63198 |
31KH19N9MVBTL ( 31Х19Н9МВБТЛ ) - Casting alloy steel with specific properties 31KH19N9MVBT ( 31Х19Н9МВБТ ) - High alloy high-temperature steel 31KH19N9MVBTL ( 31Х19Н9МВБТЛ ), 31KH19N9MVBT ( 31Х19Н9МВБТ ), |
B82 - Steel Castings |
В22 - Graded and shaped rolling |
B23 - Sheets and Strips |
В32 - Graded and shaped rolling |
B33 - Sheets and Strips |