Database of Steel and Alloy (Marochnik) |
Home | Steel and Alloy | Search | Equivalent Grades | GOST Standards | Grading | Contacts |
Country - USA | Standard - UNS | Grade - J13002 |
20G1FL ( 20Г1ФЛ ) - Casting alloy steel for general purposes 20G1FL ( 20Г1ФЛ ), |
B42 - Rails: Pads, Pads, Crutches |
B82 - Steel Castings |