Database of Steel and Alloy (Marochnik)

  Home     Steel and Alloy     Search     Equivalent Grades     GOST Standards     Grading     Contacts  
         
Equivalent grades   ->   USA. Casting steel    

Equivalents to grade H41370

    Country   -   USA         Standard   -   UNS         Grade   -   H41370    

    35KHML   ( 35ХМЛ )   -   Casting alloy steel for general purposes

  35KHML   ( 35ХМЛ ),      

35KHML   ( 35ХМЛ )   -   All Equivalent Grades
chemical composition, mechanical and technological properties

Types of delivery of grade 35KHML   ( 35ХМЛ )
B82 - Steel Castings
B83 - Castings with special properties (cast iron and steel)


H41370 USA Casting steel:   Equivalent Grades for Russia, Ukraine, Belorussia, Kazakhstan...