Database of Steel and Alloy (Marochnik) |
Home | Steel and Alloy | Search | Equivalent Grades | GOST Standards | Grading | Contacts |
Country - Germany | Standard - DIN | Grade - GS-36Mn5 |
35GL ( 35ГЛ ) - Casting alloy steel for general purposes 35GL ( 35ГЛ ), |
B82 - Steel Castings |
© 2003 - 2024 Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use. |