Equivalents to grade D5

    Country   -   USA         Standard   -   AISI         Grade   -   D5    

    KH12F1   ( Х12Ф1 )   -   Die tool steel

  KH12F1   ( Х12Ф1 ),      

KH12F1   ( Х12Ф1 )   -   All Equivalent Grades
chemical composition, mechanical and technological properties

Types of delivery of grade KH12F1   ( Х12Ф1 )
В32 - Graded and shaped rolling