Equivalents to grade T11323

    Country   -   USA         Standard   -   UNS         Grade   -   T11323    

    R6M5F3   ( Р6М5Ф3 )   -   High speed tool steel

  R6M5F3   ( Р6М5Ф3 ),      

R6M5F3   ( Р6М5Ф3 )   -   All Equivalent Grades
chemical composition, mechanical and technological properties

Types of delivery of grade R6M5F3   ( Р6М5Ф3 )
В22 - Graded and shaped rolling
В32 - Graded and shaped rolling
B33 - Sheets and Strips


T11323 USA Tool steel:   Equivalent Grades for Russia, Ukraine, Belorussia, Kazakhstan...