Country - Germany | Standard - DIN | Grade - 57NiCrMoV7-7 |
4KHMNFS ( 4ХМНФС ) - Alloy tool steel 7KH3 ( 7Х3 ) - Die tool steel 5KHGM ( 5ХГМ ) - Die tool steel 5KH2MNF ( 5Х2МНФ ) - Die tool steel 4KHMNFS ( 4ХМНФС ), 7KH3 ( 7Х3 ), 5KHGM ( 5ХГМ ), 5KH2MNF ( 5Х2МНФ ), |
В32 - Graded and shaped rolling |
В22 - Graded and shaped rolling |
B31 - Blanks, Blanks, Slabs |
В32 - Graded and shaped rolling |
B33 - Sheets and Strips |
В22 - Graded and shaped rolling |
B31 - Blanks, Blanks, Slabs |
В32 - Graded and shaped rolling |
B33 - Sheets and Strips |
В32 - Graded and shaped rolling |