Database of Steel and Alloy (Marochnik)

  Home     Steel and Alloy     Search     Equivalent Grades     GOST Standards     Grading     Contacts  
         
Equivalent grades   ->   European. Structural steel    

Equivalents to grade 102Cr6

    Country   -   European         Standard   -   EN 96         Grade   -   102Cr6    

    KH   ( Х )   -   Alloy tool steel
    SHKH15   ( ШХ15 )   -   Bearing structural steel

  KH   ( Х ),         SHKH15   ( ШХ15 ),      

KH   ( Х )   -   All Equivalent Grades
chemical composition, mechanical and technological properties

Types of delivery of grade KH   ( Х )
В32 - Graded and shaped rolling

SHKH15   ( ШХ15 )   -   All Equivalent Grades
chemical composition, mechanical and technological properties

Types of delivery of grade SHKH15   ( ШХ15 )
В22 - Graded and shaped rolling
B23 - Sheets and Strips
В32 - Graded and shaped rolling
В62 - Steel pipes and connecting parts to them
B73 - Steel Alloy Wire


102Cr6 European Structural steel:   Equivalent Grades for Russia, Ukraine, Belorussia, Kazakhstan...

    ©   2003 - 2019         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Previous address of this website was splav.kharkov.com
Рейтинг@Mail.ru