Database of Steel and Alloy (Marochnik)

  Home     Steel and Alloy     Search     Equivalent Grades     GOST Standards     Grading     Contacts  
         
Equivalent grades   ->   European. Aluminium alloy    

Equivalents to grade ENAW-1199

    Country   -   European         Standard   -   EN 573-3-94         Grade   -   ENAW-1199    

    А99   ( А99 )   -   Primary aluminium
    АDoch   ( АДоч )   -   Technical aluminium

  А99   ( А99 ),         АDoch   ( АДоч ),      

А99   ( А99 )   -   All Equivalent Grades
chemical composition, mechanical and technological properties

Types of delivery of grade А99   ( А99 )
B51 - Non-ferrous metals, including rare metals, and their alloys
B53 - Sheets and Strips

АDoch   ( АДоч )   -   All Equivalent Grades
chemical composition, mechanical and technological properties


ENAW-1199 European Aluminium alloy:   Equivalent Grades for Russia, Ukraine, Belorussia, Kazakhstan...

    ©   2003 - 2024         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru