    Country   -   Inter         Standard   -   ISO 1052-1982         Grade   -   Fe690    

    VSt6sp   ( ВСт6сп )   -   Normal quality structural carbon steel
    S375   ( С375 )   -   Steel for structural constructions

  VSt6sp   ( ВСт6сп ),         S375   ( С375 ),      

VSt6sp   ( ВСт6сп )   -   All Equivalent Grades
chemical composition, mechanical and technological properties

Types of delivery of grade VSt6sp   ( ВСт6сп )
В22 - Graded and shaped rolling
B23 - Sheets and Strips
В62 - Steel pipes and connecting parts to them

S375   ( С375 )   -   All Equivalent Grades
chemical composition, mechanical and technological properties

Types of delivery of grade S375   ( С375 )
В22 - Graded and shaped rolling
B23 - Sheets and Strips


Fe690 Inter Steel for special use:   Equivalent Grades for Russia, Ukraine, Belorussia, Kazakhstan...