Database of Steel and Alloy (Marochnik)

  Home     Steel and Alloy     Search     Equivalent Grades     GOST Standards     Grading     Contacts  
         
Equivalent grades   ->   Inter. Aluminium alloy    

Equivalents to grade E-AlMgSi

    Country   -   Inter         Standard   -   ISO 209-1         Grade   -   E-AlMgSi    

    AD31E   ( АД31Е )   -   Aluminium wrought alloys

  AD31E   ( АД31Е ),      

AD31E   ( АД31Е )   -   All Equivalent Grades
chemical composition, mechanical and technological properties

Types of delivery of grade AD31E   ( АД31Е )
B52 - Graded and shaped rolling


E-AlMgSi Inter Aluminium alloy:   Equivalent Grades for Russia, Ukraine, Belorussia, Kazakhstan...

    ©   2003 - 2024         Database of Steel and Alloy (russian title is the Marochnik)