    Country   -   USA         Standard   -   ASTM A276         Grade   -   403    

    12KH13 ( 12Х13 )   -   Corrosion-resistant high-temperature steel
    08KH13 ( 08Х13 )   -   Corrosion-resistant high-temperature steel

  12KH13 ( 12Х13 ),         08KH13 ( 08Х13 ),      