Equivalent grades   ->   Japan. High-temperature or heat-resistant steel and alloy    

Equivalents to grade SUH310

    Country   -   Japan         Standard   -   JIS G-4311         Grade   -   SUH310    

NEW !  
SteelJIS : Free database of Japanese steels and alloys
SteelJIS.com contains the information about chemical composition and properties
more than 1400 Japanese engineering materials.
  SteelJIS.com:   Japanese Steels and Alloys



    20KH23N18   ( 20Х23Н18 )   -   High alloy high-temperature steel
    20KH25N20S2   ( 20Х25Н20С2 )   -   High alloy high-temperature steel
    10KH23N18   ( 10Х23Н18 )   -   High alloy high-temperature steel

  20KH23N18   ( 20Х23Н18 ),         20KH25N20S2   ( 20Х25Н20С2 ),         10KH23N18   ( 10Х23Н18 ),      

20KH23N18   ( 20Х23Н18 )   -   All Equivalent Grades
chemical composition, mechanical and technological properties

Types of delivery of grade 20KH23N18   ( 20Х23Н18 )
В22 - Graded and shaped rolling
B23 - Sheets and Strips
В32 - Graded and shaped rolling
B33 - Sheets and Strips
B34 - Ribbons

20KH25N20S2   ( 20Х25Н20С2 )   -   All Equivalent Grades
chemical composition, mechanical and technological properties

Types of delivery of grade 20KH25N20S2   ( 20Х25Н20С2 )
В22 - Graded and shaped rolling
B23 - Sheets and Strips
В32 - Graded and shaped rolling
B33 - Sheets and Strips

10KH23N18   ( 10Х23Н18 )   -   All Equivalent Grades
chemical composition, mechanical and technological properties

Types of delivery of grade 10KH23N18   ( 10Х23Н18 )
B03 - Metal forming treatment. Forgings
В22 - Graded and shaped rolling
B23 - Sheets and Strips
В32 - Graded and shaped rolling
B33 - Sheets and Strips
В62 - Steel pipes and connecting parts to them


SUH310 Japan High-temperature or heat-resistant steel and alloy:   Equivalent Grades for Russia, Ukraine, Belorussia, Kazakhstan...