Database of Steel and Alloy (Marochnik) |
Home | Steel and Alloy | Search | Equivalent Grades | GOST Standards | Grading | Contacts |
Country - European | Standard - EN 573-3 | Grade - ENAW-AlMn1Mg0.5 |
MM ( ММ ) - Aluminium wrought alloys MM ( ММ ), |
B51 - Non-ferrous metals, including rare metals, and their alloys |
В54 - Ribbons |