Database of Steel and Alloy (Marochnik)

  Home     Steel and Alloy     Search     Equivalent Grades     GOST Standards     Grading     Contacts  


Propositions
of the Department of
Physical Engineering


NTU KhPI
National Technical University
Kharkov Polytechnic Institute




Education for foreigners in Ukraine

Russian
  Grade  

                Welcome!

              Database of Steels and Alloys  ( russian title is the Marochnik )   contains the information about classification, chemical composition, critical points, hardness by Brinell, physical, mechanical and technological properties of   3300   steels and alloys from former Soviet Union countries (Russia, Ukraine, Belorussia, Estonia, Kazakhstan ...)

             Searchable Database of steels and alloys (Marochnik) is useful for metal suppliers and purchasers, export/import departments, mechanical engineers, constructors, metallurgists, technologists, material testing departments and others who have something to do with metal.


You can visit our new project " EUROPEAN STEEL AND ALLOY GRADES / NUMBERS ".
It contains the information about more than 2100 materials from European Union.


NEW !  
SteelJIS : Free database of Japanese steels and alloys
SteelJIS.com contains the information about chemical composition and properties
more than 1400 Japanese engineering materials.
  SteelJIS.com:   Japanese Steels and Alloys



              The entire risk as to use of the Database of Steels and Alloys content is assumed by you the user. This program is not in the business of rendering engineering or structural advice. Accordingly, you shall not rely on the our materials database or its content in making structural or engineering decisions and calculations.

To copy the Database of Steels and Alloys content for public use is illegal

Database of steels and alloys (Marochnik) are only informational resource. We are not connected with any commercial activity.
Previous address of this website was splav.kharkov.com



    ©   2003 - 2022         Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use.
Рейтинг@Mail.ru