Grade : | 03KH19G10N7M2 ( 03Х19Г10Н7М2 ) |
Classification : | Сryogenic structural steel |
Equivalent grades: | Is absent |
C | Si | Mn | Ni | S | P | Cr | Mo | N |
max 0.03 | max 0.8 | 9 - 11 | 6.5 - 7.5 | max 0.025 | max 0.035 | 18.5 - 20.5 | 2 - 2.5 | 0.3 - 0.4 |
Weldability: | without limitations. |
Mechanical properties : | |
sв | - Tensile strength , [MPa] |
sT | - Yield stress, [MPa] |
d5 | - Specific elongation at fracture , [ % ] |
y | - Reduction of area , [ % ] |
KCU | - Impact strength , [ kJ / m2] |
HB | - Brinell hardness , [MPa] |
Physical properties : | |
T | - Test temperature , [Grade] |
E | - Young modulus , [MPa] |
a | - Coefficient of linear expansion (range 20o - T ) , [1/Grade] |
l | - Termal (heat) condition coefficient , [Watt/(m·Grade)] |
r | - Density , [kg/m3] |
C | - Specific heat ( range 20o - T ), [J/(kg·Grade)] |
R | - Electrical resistance , [Ohm·m] |
Weldability : | |
without limitations | - welding is done without heating and subsequent heat treeting |
limited weldability | - welding is possible under heating up to 100-120 grade and subsequent heat treeting |
hard weldability | - obtaining the quality welding needs the additional operations:heating up to 200-300 grade; the heat treeting ia annealing |