Database of Steel and Alloy (Marochnik) |
Home | Steel and Alloy | Search | Equivalent Grades | GOST Standards | Grading | Contacts |
Grade : | АCHK-1 ( АЧК-1 ) |
Classification : | Antifriction iron castings |
Equivalent grades: | Is absent |
C | Si | Mn | S | P | Cu |
2.3 - 3 | 0.5 - 1 | 0.6 - 1.2 | max 0.12 | max 0.2 | 1 - 1.5 |
Brinell hardness for АCHK-1 ( АЧК-1 ) , GOST 1585-85 | HB 10 -1 = 187 - 229 MPa |
Load | Speed | Load * Speed | Temperature |
MPa | m/s | MPa * m/s | Grade |
20 | 2 | 20 |
В81 - Castings of cast iron (gray and malleable cast iron) |
Mechanical properties : | |
sв | - Tensile strength , [MPa] |
sT | - Yield stress, [MPa] |
d5 | - Specific elongation at fracture , [ % ] |
y | - Reduction of area , [ % ] |
KCU | - Impact strength , [ kJ / m2] |
HB | - Brinell hardness , [MPa] |
Physical properties : | |
T | - Test temperature , [Grade] |
E | - Young modulus , [MPa] |
a | - Coefficient of linear expansion (range 20o - T ) , [1/Grade] |
l | - Termal (heat) condition coefficient , [Watt/(m·Grade)] |
r | - Density , [kg/m3] |
C | - Specific heat ( range 20o - T ), [J/(kg·Grade)] |
R | - Electrical resistance , [Ohm·m] |
© 2003 - 2025 Database of Steel and Alloy (russian title is the Marochnik)
Administration of the Marochnik is not responsible for the content's use. |